Ready Plastics
PEIRodNatural

Ultem 1000 (PEI) - 1.250" dia x 60 Natural Rod - 60 in Rod

60 in Rod

Ultem 1000 (PEI) - 1.250" dia x 60 Natural RodUltem 1000 (PEI) - 1.250" dia x 60 Natural Rod - view 2Ultem 1000 (PEI) - 1.250" dia x 60 Natural Rod - view 3
Same-day shipping available
Quality certified
Expert support

This PEI rod measures 1.25″ diameter × 60″ length, finished in natural. In stock — price $173.14 per Each.

SpecificationValueTolerance
Shape / FormRod
Diameter1.25Standard
Length60Standard
ColorNatural
About This Product

Ultem 1000 (PEI) Polyetherimide rod in Natural is supplied in a 1.25" diameter x 60" long size for demanding electrical, aerospace, and high-temperature machining applications. This unfilled PEI grade offers excellent heat deflection, strong dimensional stability, and inherent flame resistance, making it a reliable choice for precision parts exposed to elevated temperatures.

Specifications

Resin

Ultem 1000

Shape

Rod

Length

60 in

Outer Diameter

1.25 in

Color

Natural

Unit of Measure

Each

Other PEI sizes

← All PEIstock & specs

Price

$173.14 / Each

In Stock
21010 available
Available at 11 locations

Minimum order: 5 units

Ships same day if ordered by 2pm
Quality guaranteed
Quick Info
ResinUltem 1000
CategoryPEI
FormRod
Length60 in
Outer Diameter1.25 in

Typical Properties — Ultem 1000 (PEI) - 1.250" dia x 60 Natural Rod

Pei
General
PropertyTest MethodUnitValue
DensityD792lb/in³ / g/cm³0.046 / 1.2
Water absorption (24 / 96 h immersion @ 73°F)ASTM D570mg / %20/41 / 0.26/0.54
Water absorption (Saturation in air @ 73°F, 50% RH)ASTM D570%0.75
Water absorption (Saturation in water @ 73°F)ASTM D570%1.35
Flammability rating (UL 94, 3 / 6 mm thickness)UL 94V-0/V-0
Mechanical
PropertyTest MethodUnitValue
Tensile strength (At yield / break)ASTM D638psi / MPa15,250 / 105
Tensile strain at breakASTM D638%10
Tensile modulusASTM D638psi / MPa493,000 / 3,300
Compressive stress (At 10% nominal strain)ASTM D695psi / MPa22,000 / 150
Rockwell hardnessASTM D785R126
Operating Environment
PropertyTest MethodUnitValue
Thermal conductivity (@ 73°F)ASTM C177Btu·in/ft²·h·°F / W/m·K1.5 / 0.21
Coefficient of thermal expansion (Avg. 73 – 140°F)ASTM D696μin/in/°F / μm/m/°C25 / 45
Coefficient of thermal expansion (Avg. 73 – 212°F)ASTM D696μin/in/°F / μm/m/°C25 / 45
Heat deflection temperature (264 psi (Method A))ASTM D648°F / °C375 / 190
Max service temperature (Short-term)°F / °C390 / 195
Max service temperature (Continuous (5,000 / 20,000 h))°F / °C340 / 170
Electrical
PropertyTest MethodUnitValue
Dielectric strengthASTM D149V/mil / kV/mm685 / 26
Volume resistivityASTM D257Ω·cm>10¹⁴
Surface resistivityASTM D257Ω>10¹³

Typical properties are provided for reference only. Values may vary based on processing conditions, form factor, and lot. Contact Ready Plastics for certified test data.